3D printing powder for die casting molds
TFME 23A is a 3D printing powder used in die-casting molds. Hot-work molds operate in harsh environments, with their working surfaces subjected to cyclic stamping loads, temperature differences, and frictional wear. This can easily lead to mold wear, fracture, thermal fatigue, and cavity collapse, severely reducing the mold’s lifespan. Therefore, the surface of hot-work molds must possess excellent thermal stability and wear resistance.
TFME 23A, as a hot-work mold steel material, possesses high strength, hardness, and red hardness, while also exhibiting good thermal conductivity and high fatigue resistance. TFME 23A mold steel powder is primarily used in the 3D printing of die-casting molds.
Range of chemical composition
| C | Si | Mn | Cr | Mo | V | Bal |
|---|---|---|---|---|---|---|
| 0.25-0.30 | 0.10-0.30 | 0.30-0.50 | 4.70-5.20 | 3.00-3.50 | 0.30-0.60 | ≤3.00 |
Physical properties
| Granularity range | 15-53 µm |
|---|---|
| Hardness after heat treatment | 44-53 HRC |
| Hallflow rate | ≤18 s/50 g |
| Loose packing density | 4.2 g/cm3 |
| Heat conductivity | 34.5 W/m.K |
| Impact energy (1030°C + 615°C x 2) | 36.6 J |
| Ensile strength (1030°C + 590°C x 2) | 1649.6 MPa |
The high-temperature stability curve is as follows

Download the TMFE 23A datasheet (PDF)