Laser cladding repair of hydraulic support columns and rollers
Compared to traditional hard chrome plating, laser cladding offers metallurgical advantages. It also helps reduce overall operating costs by extending service life.
TFMS 13A is an alloy powder with good wear and corrosion resistance. Laser cladding allows for hardnesses up to 53 – 55 HRC. It is widely used in the repair of hydraulic columns and rollers.
Range of chemical composition
| C | Cr | Ni | Mo | Mn | Si |
|---|---|---|---|---|---|
| ≤0.17 | ≤17.5 | ≤2.60 | ≤1.80 | ≤0.35 | <0.8 |
Physical properties
| Granularity range | 53-150 µm |
|---|---|
| Hardness | 53-55 HRC |
| Hallflow rate | ≤18 s/ 50 g |
| Loose packing density | 4.48 g/cm3 |
Corrosion resistance test
| Neutral spray test GB / T 10125 – 2021 | 3000 |
|---|
Download the TFMS 13A datasheet (PDF)