Applications
Motor Shafts, Aircraft Structural parts, Valve Stems, Gears
Features
- The 17-4 PH is a martensitic precipitation-hardening stainless steel with excellent corrosion resistance and outstanding mechanical properties. Conforming to the stringent AMS 5604, AMS 5622, and AMS 5643 specifications, this alloy is meticulously engineered to meet the most demanding industrial requirements.
- The exceptional corrosion resistance of the 17-4 PH alloy stems from its carefully crafted chemical composition, blending chromium, nickel, and copper in precise proportions, this unique formulation imbues the material with an unrivaled ability to withstand a broad spectrum of corrosive environments.
- Moreover, the alloy’s precipitation hardening capabilities allow for precise control over its mechanical properties, through a carefully controlled heat treatment process, 17-4 PH can achieve remarkable strength and hardness levels while maintaining excellent toughness and ductility.
Standard
AMS 5604 / AMS 5622 / AMS 5643
Material
17-4 PH / UNS S17400 / W.Nr 1.4548
Chemical composition (Nominal) %
| Grade | C | Mn | Si | P | S | Cr |
|---|---|---|---|---|---|---|
| 17-4 PH | 0.07 max | 1.00 max | 1.00 max | 0.040 max | 0.030 max | 15.00-17.50 |
| Ni | Nb | Cu | Mo | Fe |
|---|---|---|---|---|
| 3.00-5.00 | 5xC%-0.45 | 3.00-5.00 | 0.50 max | Bal |
Physical properties
| Density | 7.74 g/cm3 |
|---|
Mechanical properties
| Condition | Tensile Strength, min, MPa | Yield Strength, min. (0.2 % offset), min, MPa | Elongation in 2 in. or 50 mm (or 4D), % | Reduction of Area, min,% | Hardness, HB | Hardness, HRC |
|---|---|---|---|---|---|---|
| H900 | 1310 | 1172 | 10 | 40 | 388-444 | 40-47 |
| H925 | 1172 | 1069 | 10 | 44 | 375-429 | 38-45 |
| H1025 | 1069 | 1000 | 12 | 45 | 331-401 | 34-42 |
| H1075 | 1000 | 862 | 13 | 45 | 311-375 | 31-38 |
| H1100 | 965 | 793 | 14 | 45 | 302-363 | 30-37 |
| H1150 | 931 | 724 | 16 | 50 | 277-352 | 28-37 |
Round bar
Size range
| Product | Material | WD Range | Length Range |
|---|---|---|---|
| ROUND BAR | 17-4 PH | Φ5mm ~ Φ500mm | 3000~6000mm |
Plate and sheet
Size range
| Product | Material | WD Range | Length Range | WT Range |
|---|---|---|---|---|
| PLATE & SHEET | 17-4 PH | 1000~2000mm | 2000~6000mm | 0.5~150mm |